Detection of internal wall reduction artifacts in manufactured pipe.

Background

Localized wall reductions are not always caused by corrosion. Wall reductions can develop during plate rolling or the initial stages of forming in the pipe manufacturing process. Impressions in the steel can be created by the forming rollers. High surface pressure and heat applied to the forming rollers can induce spalling. Metal pieces that spall and become detached from the rollers can fall into the path of the incoming plate causing the pieces to bond to the roller. Once the pieces are bound to the roller, impressions begin occurring in the plate being rolled. Hence the term artifacts from the impression caused by the roller, which appear similar to be wall reductions caused by corrosion.

In many cases new pipe is put into service with such artifacts. When corrosion inspection is later performed after he pipe has been in operation, inspectors may find these wall reduction artifacts and mistake them for corrosion cells. If this occurs, process engineers may infer an incorrectly fast corrosion rate and make incorrect process changes and or chemical additives. However a simple ultrasonic gaging procedure can identify artifacts at the manufacturing or installation stage.

Equipment

Model 38DLP PLUS thickness gage, or Model 45MG gage with waveform display option, and D790 dual element transducer (5 MHz).

Example

The pipe in the picture below is 8” x .250” wall carbon steel 1018 grade manufactured with the ERW process. The dark indentions are artifacts reducing wall thickness that occurred during the pipe forming process. No corrosion was present on the ID or OD.

The pipe in the picture below is 8” x .250” wall carbon steel 1018 grade manufactured with the ERW process

Thickness gaging is performed in the same manner as a corrosion survey. In the picture at left, the gage is reading full wall thickness. In the picture at right, the thinner reading indicates a wall thinning artifact on the inside surface.

The gage is reading full wall thickness
The thinner reading indicates a wall thinning artifact on the inside surface.

An inspector may consider the following factors when attempting to distinguish manufacturing artifacts from corrosion cells:

Conclusion

Manufacturing artifacts in pipe can be detected by ultrasonic thickness gaging. Inspectors performing thickness measurement of piping should be aware of this damage mechanism. It is also important to inform the process plant quality control inspectors of this potential problem to avoid over-estimating corrosion rates.

Prodotti per l'applicazione

45MG

L'innovativo misuratore di spessori a ultrasuoni 45MG integra delle funzionalità di misura di serie e delle opzioni software. Questo eccezionale strumento di misura di spessore è compatibile con la nostra completa gamma di trasduttori per misuratori di spessori a singolo o doppio elemento.

38DL PLUS

Il versatile misuratore 38DL PLUS™ può essere usato in combinazione con i trasduttori a doppio elemento in diversi ambiti: dalla misura di tubazioni corrose mediante trasduttori a doppio elemento, alla misura molto precisa di spessori di componenti sottili in materiale multistrato mediante trasduttori a singolo elemento.